[口头报告]Experimental Study on Leakage Plugging and Coal Self-heating Inhibition of the Thermo-responsive Secundina Sphere Inhibitor

Experimental Study on Leakage Plugging and Coal Self-heating Inhibition of the Thermo-responsive Secundina Sphere Inhibitor
编号:213 稿件编号:191 访问权限:仅限参会人 更新:2024-05-15 17:43:49 浏览:587次 口头报告

报告开始:2024年05月31日 17:00 (Asia/Shanghai)

报告时间:10min

所在会议:[S2] Safety Engineering and Occupational Health » [S2-3B] Afternoon of May 31st B

暂无文件

摘要
This paper comprehensively analyzes the permeation plugging and coal self-heating inhibition of the thermo-responsive secundina sphere inhibitor (TRSSI) composed of a phase change shell and an internal saltwater inhibitor. Experimental setups included a coal sample leak-blocking device and a coal self-heating adiabatic oxidation platform. The inhibitor's inhibition mechanism was studied using infrared spectroscopy (FTIR) and scanning electron microscopy (SEM). Results indicate that smaller particle sizes enhance the bonding of the shell phase change material to coal particles, improving air blocking. In a condensed coal sample with a 1-3mm particle size, the pressure difference at both ends is 1.4 times higher than in a loose coal sample. The TRSSI exhibited significant inhibition effects throughout the coal self-heating process. Initially, the TRSSI's shell absorbs the heat from the coal, causing the TRSSIs to deform and accumulate on the coal surface. This process effectively slows down the rate at which the coal surface heats up. At the same heat source temperature, the heating rate of the raw coal sample is 4.02 ℃/d, while the heating rate of the inhibition coal sample is only 2.35 ℃/d. Later, the TRSSI released a sufficient amount of internal inhibitor liquid that precisely acted on the center of the coal seam heat source, causing the heat source temperature to drop from 180 ℃ to 50 ℃ rapidly. Microscopic analysis revealed a decrease in oxygen-containing groups, hydrocarbons, and -C=C in inhibited coal samples, making self-ignition more challenging. Furthermore, the TRSSI's shell envelops the coal seam post phase change, delaying self-thermal oxidation by isolating coal from oxygen contact.
关键字
Thermo-responsive; coal; low temperature oxidation; inhibition
报告人
Chenchen Yin
China university of mining and technology

稿件作者
Chenchen Yin China university of mining and technology
Shuguang Jiang China University of Mining and Technology
Zhengyan Wu China University of Mining and Technology
Xian Xi China University of Mining and Technology
发表评论
验证码 看不清楚,更换一张
全部评论

联系我们

投稿事宜:张老师
电话:0516-83995113
会务事宜:张老师
电话:0516-83590258
酒店事宜:张老师
电话:15852197548
会展合作:李老师
电话:0516-83590246
登录 注册缴费 提交摘要 酒店预订